Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® A3HG2 - PA66-GF10 - BASF

Material Data Center offers the following functions for Ultramid® A3HG2:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultramid A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 80 / * cm³/10min ISO 1133
Temperature 275 / * °C -
Load 5 / * kg -
ASTM Data
Mold Shrinkage, MD 0.008 mm/mm ASTM D 955
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 4600 / 2600 MPa ISO 527
Stress at break 100 / 60 MPa ISO 527
Strain at break 2.8 / 12 % ISO 527
Flexural modulus, 23°C 4600 / - MPa ISO 178
Charpy impact strength, +23°C 30 / 92 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 7 / 9 kJ/m² ISO 179/1eA
Izod notched impact strength, +23°C - / 7 kJ/m² ISO 180/1A
ASTM Data
Tensile Strength at Break 100 / - MPa ASTM D 638
Elongation at Break 3 / - % ASTM D 638
Flexural Modulus 4480 / - MPa ASTM D 790
Izod Impact notched, 1/8 in 53 / - J/m ASTM D 256
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 260 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 210 / * °C ISO 75-1/-2
Burning behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.6 / * mm -
ASTM Data
DTUL @ 264 psi 210 °C ASTM D 648
Melting Temperature 260 °C ASTM D 3418
Electrical propertiesdry / condUnitTest Standard
ISO Data
Relative permittivity, 1MHz 3.5 / 5.5 - IEC 62631-2-1
Dissipation factor, 1MHz 140 / 1600 E-4 IEC 62631-2-1
Volume resistivity 1E13 / 1E10 Ohm*m IEC 62631-3-1
Surface resistivity * / 1E10 Ohm IEC 62631-3-2
Comparative tracking index 550 / - - IEC 60112
ASTM Data
Volume Resistivity 1E13 / - Ohm*cm ASTM D 257
Other propertiesdry / condUnitTest Standard
Water absorption 7 / * % Sim. to ISO 62
Humidity absorption 2.1 / * % Sim. to ISO 62
Density 1200 / - kg/m³ ISO 1183
Water Absorption, Equilibrium 7 % ASTM D 570
Density 1200 kg/m³ ASTM D 792
Material specific propertiesdry / condUnitTest Standard
ISO Data
Viscosity number 148 / * cm³/g ISO 307, 1157, 1628
Characteristics
Processing
Injection Molding, Other Extrusion
Delivery form
Pellets
Applications
Automotive, Electrical and Electronical
Regional Availability
Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.